Sunday, 12 March 2017

Door skin and sill.

Inside door skin coated in wax treatment.






 Outer sill all plug welded on by Owen.


 Looking nice Owen well done.

Passenger side outer sill

Taped off and sprayed in a coating of wax protection helping against rust.


After a fairly thick layer of wax protection and 12hr later the wax was pretty much dry.


Whilst I was dirtying the spray gun anyway I thought I would coat the inner door skins
 and outer sills leaving an area coated in weld through primer along the seem .


Outer sills were drilled ready for plug welding and the area cleaned
where the sills were to be welded. 


Owen cracked on with the preparation.